MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Rando® HD 46
Categories: Fluid; Lubricant

Material Notes: Texaco Rando HD oils deliver value through:
  • Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.
  • Reduced downtime — Effective rust and oxidation inhibitor system prevents the production of abrasive particles from rust formation, and deposits, varnishes and sludges from oil breakdown, which can damage equipment surfaces and seals, and block filters prematurely.
  • Trouble-free operation — Good hydrolytic stability and water separation characteristics provide excellent filterability in the presence of water contamination. Good anti-foam and air release properties ensure smooth operation and system efficiency.
  • Extended oil service life — High oxidation stability resists oil thickening and deposit formation in service, eliminating the need for unscheduled change of hydraulic fluid.

Texaco Rando HD ISO 32, 46, and 68 are designed to give maximum hydraulic pump protection in mobile and stationary systems.

Texaco Rando HD ISO 100, 150, and 200 are designed for all types of lubricant applications where a premium antiwear lubricant in their ISO viscosity grade is required, such as an AGMA Gear Lubricant or general machinery lubrication.

Texaco Rando HD oils provide excellent:

  • Antiwear protection
  • Oxidation and corrosion inhibition
  • Foam and aeration suppression

Under moderate loads and temperatures, the high viscosity index of Texaco Rando HD oils assures good film strength between metal surfaces and is further enhanced by antiwear additive protection.

Texaco Rando HD ISO 32, 46, or 68 are recommended for:

  • Vane-, piston-, or gear-type pumps, especially where pressures exceed 1000 psi
  • Lightly loaded reciprocating compressors
  • Motors and bearings.

Texaco Rando HD ISO 100, 150, or 220 are recommended for:
  • Hydraulic equipment reduction gears
  • Reciprocating air compressors
  • Plain and antifriction bearings
  • Circulating oil systems

Texaco Rando HD oils meet the requirements of:
  • Vickers I-286-S, M-2950-S, 35VQ-25 (ISO 32, 46, 68)
  • Cincinnati Machine P-68 (ISO 32), P-70 (ISO 46), P-69 (ISO 68)
  • Denison HF-0/T6C, HF-2 (ISO 32, 46, 68)
  • ANSI/AGMA 9005-D94, Industrial Gear Lubrication, for gear lubrication as rust and oxidation inhibited gear oils (ISO 46, 68, 100, 150, 220)
  • the U.S. Department of Agriculture (USDA) as H2 lubricants for use in federally inspected meat and poultry plants where no food contact will occur. (ISO 32, 46, 68, 150, 220)

Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221658; MSDS Number: 8643

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D943, Hours to 2 mg KOH/g acid number
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.