MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® DX9323 BK E70228 Nylon 612, 35% Glass Fiber Reinforced, Impact Modified, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler; Nylon 612, Impact Modified

Material Notes: VESTAMID® DX9323 BK E70228 is a heat-stabilized, glass fiber-reinforced and impact-modified PA 612 compound. The material contains about 35% glass fiber, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9323 BK E70228 is especially suitable for the production of plastic and rubber composites. Parts of VESTAMID® DX9323 BK E70228 can be directly bonded to rubber, e. g., XNBR, HNBR, AEM or FPM, without using any adhesives or adhesion promoters ("direct-bonding to rubber"). Because of its semi-crystalline morphology VESTAMID® DX9323 BK E70228 provides an excellent chemical resistance, e. g., against greases, oils, fuels and hydraulic fluids. VESTAMID® DX9323 BK E70228 is supplied as cylindrical pellets ready for processing in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Glass fibers, Release agent
Processing: K&K process
Special Characteristics: High impact strength, Semi-crystalline, High heat resistant
Additives: Antioxidant agent, Release agent, Impact resistant, Heat stabilizer, Processing aids
Color: Black
Additives: Oil resistance, Fuel resistance, General chemical resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, Sim to ISO 62
  • Moisture Absorption, Sim to ISO 62
  • Viscosity Number, ISO 307, 1157, 1628, Corrected
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Ash, ISO 3451
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Elongation at Break, ISO 527, nom. strain at br., etB
  • Tensile Modulus, ISO 527
  • Charpy Impact Unnotched, ISO 179/1eU, Type of failure: C
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Volume Resistivity, IEC 62631-3-1, ?V
  • Surface Resistance, IEC 62631-3-2, RSD
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Constant, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1
  • Comparative Tracking Index, IEC 60112, test solution A, 50 drops value
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50 K/h
  • Flammability, UL94, IEC 60695-11-10
  • Flammability, UL94, IEC 60695-11-10
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294, Injection Molding
  • Moisture Content, ISO 15512
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.