MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Bisalloy Steels Wear 500 Plus Steel, 8 - 40 mm
Categories: Metal; Ferrous Metal

Material Notes: BISALLOY® WEAR 500 PLUS has improved impact toughness and is through hardened. It has very high abrasion-resistance with guaranteed impact toughness at low temperature and is still readily weldable and formable for a range of applications.

Applications: Being through hardened with a nominal hardness of 500 HBW, BISALLOY® Wear 500 PLUS has been developed for highly demanding applications and can offer an increased life expectancy in sliding and gouging abrasion situations. BISALLOY® Wear 500 PLUS is best suited to applications such as:

  • Dump Truck High Impact Zones
  • Ground Engaging Tools
  • Rock Buckets and Crushers
  • Cutting Edges
  • Rock Buckets
  • Wear Liners
  • Chutes

Information provided by Bisalloy Steels Group Limited.

Vendors:
Available Properties
  • Hardness, Brinell
  • Tensile Strength
  • Tensile Strength, Yield
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.