MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Barlog Plastics KEBATER PBT A9045 black 9094 PBT+PET, 45% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PBT/PET-Blend, 45% glass fiber reinforced, optimized surface quality, improved weld line strength and reduced tendency to warp. The KEBATER PBT A9045 black 9094 color setting meets all requirements for worldwide use in contact with foodstuffs (EU 10/2011, FDA, Mercosur, China, Japan).

Properties: dimensionally stable, good chemical resistance, Good electrical properties, good gliding properties, good aging behavior, High strength, High stiffness, High wear resistance, semi-crystalline, approved for food contact use worldwide (EU 10/2011; FDA; Mercosur; China; Japan), approved for food contact (EU and FDA)

Typical areas of application: Sports & Leisure Articles, Plug, Controls, Structural components, Fasteners, Carrier, Hardware, Connecting elements, Actuating elements, Cover, Pressure cans, Housing, Handles, industrial goods, Coffee machines, media-carrying components, Pumps and motors, Pump housing, Switch

Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Agriculture, Food processing industry, Mechanical Engineering, Medical Technology, Sanitary industry

Information provided by BARLOG plastics GmbH.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Moisture Absorption, ISO 62, 50% RH
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527-1
  • Elongation at Break, ISO 527-1
  • Modulus of Elasticity, ISO 527-1
  • Charpy Impact Unnotched, ISO 179-1eU
  • Charpy Impact, Notched, ISO 179-1eA
  • Electrical Resistivity, IEC 60093, Contact
  • Surface Resistance, IEC 60093
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Flammability, UL94, IEC 60695-11-10
  • Melt Temperature
  • Mold Temperature
  • Back Pressure
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
BARLOG plastics GmbH

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.