Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
GEHR Plastics PA 6.6 Nylon 6.6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing. In addition, this conditioning occurs with a longer storage in air automatically. This polyamide has the highest hardness, rigidity, and a good resistance to wear and heat deflection temperature.

Properties:

  • high impact strength and stiffness
  • high impact and notching impact strength
  • high heat deflection temperature
  • good at dampening
  • good glide and limp home characters
  • good chemical stability against organic solvents and fuels
  • size alteration by humidity absorption must be considered
  • dimension stability, electrical and mechanical properties may become affected by absorbing moisture or water
Applications include bearing parts, gear wheels, pump parts, sliding rails, castors, and fittings.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62
  • Water Absorption at Saturation, ISO 62
  • Hardness, Shore D, ISO 868
  • Ball Indentation Hardness, ISO 2039
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Strength, ISO 178
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Coefficient of Friction, DIN 53375
  • Volume Resistivity, VDE 0303
  • Surface Resistivity per Square, VDE 0303
  • Dielectric Strength, VDE 0303
  • Dielectric Loss Index, DIN 53483
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, DIN 53752
  • Thermal Conductivity, DIN 52612
  • Melting Point, DIN EN ISO 3146
  • Maximum Service Temperature, Air, UL746B
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, DIN EN ISO 3146
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.