MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Sandvik Bioline 20AP Precision Wire
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: Sandvik Bioline 20AP is a hardenable, free-cutting carbon steel combining excellent machining properties, high hardness and dimensional stability during hardening. Very suitable for long narrow components with tight tolerances such as shafts, dental burrs and other fine mechanical components.

Service temperature -50 to +100 °C. Prolonged service at elevated temperatures causes decreased hardness when used in the hardened and tempered condition.

Information provided by Sandvik

Vendors:
Available Properties
  • Density
  • Hardness, Vickers, HV5, 600°C-tempering temperature
  • Hardness, Vickers, HV5, 100°C-tempering temperature
  • Tensile Strength, Ultimate, drawn, coiled
  • Tensile Strength, Ultimate, drawn/ground, straight
  • Tensile Strength, Ultimate, drawn, coiled
  • Tensile Strength, Ultimate, drawn, straight
  • Tensile Strength, Ultimate, Drawn/ground
  • Tensile Strength, Ultimate, Drawn/ground
  • Tensile Strength, Ultimate, Drawn
  • Tensile Strength, Ultimate, drawn, straight
  • Tensile Strength, Yield, d=1.60-2.5, drawn, coiled
  • Tensile Strength, Yield, drawn/ground, straight
  • Tensile Strength, Yield, drawn, straight
  • Tensile Strength, Yield, drawn, coiled
  • Tensile Strength, Yield, drawn/ground, straight
  • Tensile Strength, Yield, drawn/ground, straight
  • Tensile Strength, Yield, drawn, straight
  • Tensile Strength, Yield, drawn, straight
  • Elongation at Break, drawn, straight
  • Elongation at Break, drawn, coiled
  • Elongation at Break, drawn, straight
  • Elongation at Break, drawn/ground, straight
  • Elongation at Break, drawn/ground, straight
  • Elongation at Break, drawn, coiled
  • Elongation at Break, drawn, straight
  • Elongation at Break, drawn/ground, straight
  • Charpy Impact, 200°C tempering temperature
  • Charpy Impact, 300°C tempering temperature
  • Charpy Impact, 400°C tempering temperature
  • Charpy Impact, 500°C tempering temperature
  • Charpy Impact, 600°C-tempering temperature
  • Electrical Resistivity, cold drawn
  • Electrical Resistivity, heat treated
  • CTE, linear, cold drawn or heat treated
  • CTE, linear, Cold drawn
  • CTE, linear, Heat treated
  • CTE, linear, cold drawn or heat treated
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Lead, Pb
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.