MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Syncon® EP Heavy Duty Grease NLGI 1
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-viscosity, synthetic base oil and excellent EP and antiwear additives provides superior load-carrying abilities, along with an operating temperature range of -30°F to 375°F (-34°C to 190°C). Extremely effective antiwear and EP additives provide a Timken OK load of 75 lbs. Conoco Syncon EP Heavy Duty Grease is specifically recommended for: King pins; Ball, roller, needle, antifriction and sleeve bearings; Wheel bearings and universal joints; General chassis lubrication; Pillow blocks and fifth wheels; Applications where normal greases fail under extreme load; Harsh, dirty, wet environments.

This grease is oxidation inhibited, rust inhibited, corrosion inhibited, contains extreme pressure additive and an antiwear additive.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors:
Available Properties
  • Viscosity Measurement, ASTM D-2270, Viscosity Index (Base Oil Property)
  • Saybolt Viscosity at 100°F, Base Oil Property
  • Saybolt Viscosity at 210°F, Base Oil Property
  • Kinematic Viscosity at 40°C (104°F), Base Oil
  • Kinematic Viscosity at 100°C (212°F), Base Oil
  • Four Ball Extreme Pressure, Load Wear Index, USS Method
  • Four Ball Extreme Pressure, Weld Load, ASTM D-2596
  • Four Ball Wear, ASTM D-2509
  • Penetration P(60), 1/10 mm, ASTM D217
  • Timken Test, ASTM D-2596
  • Pour Point, ASTM D-97, (Base Oil Property)
  • Flash Point, ASTM D-92, (Base Oil Property)
  • Dropping Point, ASTM D-2265
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.