MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Pyrotek Pyrocast 220HT Refractory Castable
Categories: Ceramic; Carbide; Oxide; Silicon Oxide

Material Notes: Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.

Applications

  • Transfer troughs
  • Launder linings
  • Filter boxes
  • Pins and spouts

Advantages

  • Thermal shock resistance
  • High strength and erosion resistance
  • High service temperature
  • Non-wetting in continuous aluminum casting applications
  • Non-wetting to aluminum alloys that contain high levels of Mg, Zn and Si

Information provided by Pyrotek.

Vendors:
Available Properties
  • Density
  • Modulus of Rupture, ASTM C133-84
  • Compressive Strength, cured at 725°C, based on ASTM C133-84
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Processing Temperature, Recommended for use in continuous casting applications
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Pyrotek, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.