MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Mitsubishi PC-ABS 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC-ABS is an incredibly strong filament with an even higher impact resistance than regular ABS. This is a consequence of the addition of the proper amount of polycarbonate in this modification, which also creates an early perfect interlayer adhesion and a beautiful surface gloss. The above features, combined with a highly stable printing process makes PC-ABS the perfect material for mechanical parts and tools, which should be light and strong and show minimal wear after prolonged use.

Features:

  • Improved interlayer adhesion
  • High impact resistance
  • High surface gloss
  • Stable printing process
Colors: M-ABS is available from stock in 12 colors. Other colors on request

Information provided by Mitsubishi Chemical.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Filament Diameter, Tolerance: 50 µm, =95% Roundness
  • Filament Diameter, Tolerance: 100 µm, =95% Roundness
  • Melt Flow, ISO 1133
  • Storage Temperature
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527, (E)
  • Charpy Impact, Notched, ISO 179
  • Melting Point, ISO 294
  • Maximum Service Temperature, Air, ISO 75, Heat Deflection Temperature
  • Processing Temperature, Printing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.