MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly suited for applications where drastic coolants are used, or where gross cracking resistance is a concern.

Information provided by Crucible Industries

Key Words: AISI H11
Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C, air cooled from 1850°F then tempered
  • Hardness, Rockwell C, air cooled from 1850°F then tempered
  • Hardness, Rockwell C, air cooled from 1850°F then tempered
  • Hardness, Rockwell C, air cooled from 1850°F then tempered
  • Hardness, Rockwell C, air cooled from 1850°F then tempered
  • Modulus of Elasticity
  • Charpy Impact, V-notch, air cooled from 1850°F then tempered
  • Charpy Impact, V-notch, air cooled from 1850°F then tempered
  • Charpy Impact, V-notch, air cooled from 1850°F then tempered
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Processing Temperature, Critical Thermal Treatment Temperature
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, as balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.