| KYDEX® P88 is a proprietary, high performance thermoplastic profile extrusion compounds designed for use in mass transit interior applications for subways, vans buses and trains. P88 meets the Federal Transit Administration (FTA) and the Federal Rail Administration (FRA) requirements for smoke emission and flammability as tested under ASTM E662 and ASTM E162. It is the ideal thermoplastic to solve your mass transportation needs. Suggested Application: - Extruded trim pieces to cover seams or exposed edges when mating or joining KYDEX® thermoplastic components
Features: - Meets flame spread and smoke development requirements listed in 49 CFR 238
- Easy to clean graffiti/spray paint, lipstick, pen, grease and grime with cleaners such as Soft Scrub®, Fantastik®, and citrus based cleaners such as Citri Kleen HD® (avoid ammoniated cleaners)
- Resistant to a wide range of concentrated chemicals and solvents, withstands frequent cleaning without staining for fading.
Information provided by SEKISUI KYDEX, LLC. |