Polypropylene random copolymer. Titanpro SM798N is a high flow and clarified grade designed for high transparency thin wall articles. It complies with the U.S. Food and Drug Administration (FDA) regulation as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. TSCA Registry: CAS# 9010-79-1 Applications: High transparency thin walled containers, storage containers. Advantages: Excellent clarity, good surface finish and color, cycle time reduction with low processing melt temperature, good dimensional stability, good balance of rigidity and impact resistance. Fabrication: Equipment – injection molding machine; Techniques - standard processing Information provided by Lotte Advanced Materials. |