MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
CHT Group AS1803 1-Part neutral thermally conductive adhesive Sealants
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: AS1803 is a non-corrosive, 1-part, room temperature vulcanising (RTV) silicone rubber. It is one of a new family of products called acetone cure sealants that are solvent free. It exhibits excellent primerless adhesion to many substrates. The product cures rapidly in contact with atmospheric moisture to a tough rubber. AS1803 does not corrode copper or its alloys and exhibits excellent primerless adhesion when fully cured.

Key Features:

  • Good thermal conductivity
  • Non-corrosive
  • Fast skinning
  • Low linear shrinkage
  • Will meet the requirements of UL 94 V-0

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Specific Gravity, BS 903 Part A1, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Brookfield Viscosity, measured at 23+/-2°C and 65% relative humidity
  • Linear Mold Shrinkage, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Hardness, Shore A, ASTM D 2240-95, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Tensile Strength, BS903 Part A2, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Elongation at Break, BS903 Part A2, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Adhesive Bond Strength, ASTM D1002, Overlap Shear Strength, Stainless Steel 304
  • Adhesive Bond Strength, ASTM D1002, Overlap Shear Strength, Copper
  • Adhesive Bond Strength, ASTM D1002, Overlap Shear Strength, Aluminum
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • CTE, linear, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Thermal Conductivity, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Maximum Service Temperature, Air, AFS 1540B, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Minimum Service Temperature, Air, after 7 days cure at 23+/-2°C and 65% relative humidity
  • Cure Time, 65% relative humidity
  • Cure Time, Cure Through, 23+/-2°C and 65% relative humidity
  • Tack-Free Time, 23+/-2°C and 65% relative humidity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.