MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technology with a variety of polymers to produce high performance SHINSTRA compound. SHINSTRA compounds are designed by alloying engineering thermoplastics or mineral reinforcing or fiber reinforcing or hybrid filler reinforcing. SHINSTRA are tailored to control the mechanical and physical properties according to its application or customer demand. SHINSTRA are often used to replace metal parts.

    Feature and Benefits
  • Excellent impact resistance
  • High scratch resistance
  • Outstanding abrasion resistance
  • Excellent chemical resistance
  • Excellent mechanical properties
  • Improved thermal properties
  • Easy processing
  • Lighter weight
  • Cost effective

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors:
Available Properties
  • Specific Gravity
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Strength
  • Flexural Modulus
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.