| MPB-D50A is a versatile polyurethane casting resin system designed for general-purpose molding applications, offering an exceptional balance of performance and processing ease. Formulated with MDI/polyether base components that are liquid at room temperature, eliminating the need for preheating and ensuring smooth, hassle-free mixing and pouring. The mixture of the two components cures to solid at room temperature. Once cured, MPB-D50A delivers outstanding mechanical properties, including excellent tensile strength, tear resistance, and stability in wet conditions placing it ahead of many other MDI/polyether urethane systems that cure at room temperature. This makes it an ideal choice for manufacturers seeking a reliable, easy-to-use solution that doesn't compromise on durability or performance. Part-A Component: MPN-033 Part-B Component: BNA-005DFS9 Mixing Ratio: 100: 15 = Part-A: Part-B by Weight (100: 14 by Volume) Information provided by Northstar Polymers |