Features: Magnetic polystyrene nanosphere has uniform particle size, smooth surface, excellent hydrophobicity and non-biodegradability. It won't dissolve or swell in general solvent, which is conducive for application and recycling. It has strong binding ability with proteins, dyes, affinity ligands and other substances. It has large specific surface area and strong absorbability and condensability, which is suitable for the fixed carrier of some substances. Application: Magnetic polystyrene nanospheres can be widely used in chromatography, microscopy, cytography, tissue separation, cancer treatment and DNA technology. Information provided by Matexcel |