MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Reynolds EpoxAmite® 100; Hardener: 103 Slow Liquid epoxy system
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: EpoxAmite™ 100 Epoxy Laminating System is an easy-to-use liquid epoxy system formulated for a wide variety of fabrication applications. EpoxAmite™ 100 Laminating System is unfilled, low in viscosity, odorless and cures at room temperature. Cured epoxy displays exceptional physical and performance properties. It can be sanded, shaped, machined, drilled, tapped and painted. EpoxAmite™ 100 Laminating System can be used with reinforcements such as S-Glass, E-Glass, Kevlar and Carbon fibers for lay-up applications or composite parts. EpoxAmite™ 100 Resin can also be mixed with fillers such as fumed silica for gel coat applications. Urefil™ 3, Urefil™ 7 and other fillers can be added for fairing, filleting or bonding applications.

Applications:

  • Wet Lay-Up Lamination
  • General Bonding & Repair
  • Clear Coating
  • Gel Coating
  • Barrier Coating
  • Thin-Section Casting
  • Water Proofing
  • Patching & Small Laminates
Advantages Include:
  • Convenient Mix Ratios - Easy-to-Use
  • Excellent Moisture Resistance - Low Viscosity
  • Non-blush Formula - Easy-to-Mix & Apply
  • Exceptional Physical & Performance Properties

Information provided by Reynolds Advanced Materials

Vendors:
Available Properties
  • Specific Gravity, ASTM D-1475
  • Viscosity, ASTM D-2393, Mixed
  • Hardness, Shore D, ASTM D-2240
  • Tensile Strength, Ultimate, ASTM D-638, after 7 days at 73°F/23°C.
  • Tensile Strength, Ultimate, ASTM D-638, testing conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C
  • Elongation at Break, ASTM D-638
  • Tensile Modulus, ASTM D-638
  • Flexural Strength, ASTM D-790, after 7 days at 73°F/23°C.
  • Flexural Strength, ASTM D-790, testing conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C
  • Flexural Modulus, ASTM D-790
  • Compressive Strength, ASTM D-695
  • Compressive Modulus, ASTM D-695
  • Maximum Service Temperature, Air, ASTM D-648, Heat Deflection Temperature
  • Cure Time, Thin Film Working Time
  • Cure Time
  • Pot Life, ASTM D-2471
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.