MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Mitsubishi Chemical Advanced Materials Altron™ LSG PC Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Life Science Grade PC stock shapes, made from unfilled PC resin. Pre-assessed for biocompatibility on stock shape for up to 24 hours contact with body tissue according to USP VI and ISO 10993 and wetted contact applications in bioprocessing. Outstanding impact resistance, toughness, and dielectric properties, as well as very good mechanical and thermal properties. Good resistance to sterilization via EtO, plasma, gamma- & X-ray irradiation. Not suitable for steam sterilization.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption at Saturation, ASTM D570 (17)
  • Hardness, Rockwell M, ASTM D785
  • Hardness, Shore D, ISO 868
  • Tensile Strength, ISO 527-1/-2 (7)
  • Elongation at Yield, ISO 527-1/-2 (7)
  • Flexural Strength, ISO 178 (12)
  • Compressive Yield Strength, ISO 604 (10)
  • Compressive Yield Strength, ISO 604 (10)
  • Compressive Yield Strength, ISO 604 (10)
  • Shear Strength, ASTM D732
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Surface Resistivity per Square, ANSI/ESD STM 11.11
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dielectric Strength, IEC 60243-1 (15)
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM E-831 (TMA)
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous Use Temperature in Air after 20000 hr
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, DMA- Tan d
  • USP Class VI
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Mitsubishi Chemical Advanced Materials (former Quadrant Engineering Plastics Products)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.