MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Park Aerospace Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applications that require optimum signal integrity and precise impedance control, while maintaining high reliability through CAF and thermal resistance.

Key Features and Benefits:

  • Lead-Free Assembly Compatible
  • Tg >210ºC, outstanding thermal, electrical and signal loss properties
  • CAF Resistant
  • Signal Integrity and Buried Capacitance™ Options
  • High-Tg FR-4 processing
  • Available in a variety of constructions

Applications/Qualifications:

  • Fine-Line Multilayers
  • Backplanes
  • Surface-Mount Multilayers
  • BGA Multilayers
  • MCM-Ls
  • CSP Attachment
  • Wireless Communications Infrastructure
  • High Speed Services
  • High Speed Storage Networks
  • Internet Switching / Routing Systems

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors:
Available Properties
  • Density, 50% Resin Content; Internal Method
  • Water Absorption, IPC-TM-650.2.6.2.1
  • Modulus of Elasticity, ASTM D3039, Y
  • Modulus of Elasticity, ASTM D3039, X
  • Poissons Ratio, ASTM D3039, Y
  • Poissons Ratio, ASTM D3039, X
  • Peel Strength, IPC-TM-650.2.4.8, after solder float
  • Peel Strength, IPC-TM-650.2.4.8.2a, at elevated temperature
  • Peel Strength, IPC-TM-650.2.4.8, after exposure to process solutions
  • Volume Resistivity, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Volume Resistivity, IPC-TM-650.2.5.17.1, E - 24/125
  • Surface Resistance, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Surface Resistance, IPC-TM-650.2.5.17.1, E - 24/125
  • Dielectric Constant, Split Post Cavity
  • Dielectric Constant, IPC-TM-650.2.5.5.5, Stripline
  • Dielectric Constant, Split Post Cavity
  • Dielectric Constant, IPC-TM-650.2.5.5.9, RF Impedance
  • Dielectric Strength, IPC-TM-650.2.5.6.2
  • Dielectric Breakdown, IPC-TM-650.2.5.6
  • Dissipation Factor, Split Post Cavity
  • Dissipation Factor, Split Post Cavity
  • Dissipation Factor, IPC-TM-650.2.5.5.5, Stripline
  • Arc Resistance, IPC-TM-650.2.5.1
  • CTE, linear, IPC-TM-650.2.4.41, X/Y
  • CTE, linear, IPC-TM-650.2.4.41, Z-Axis Alpha 1
  • CTE, linear, IPC-TM-650.2.4.41, Z-Axis Alpha 2
  • Specific Heat Capacity, ASTM E1461
  • Thermal Conductivity, ASTM E1461
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24c, TMA
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.25c, DSC
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24.3, DMA (Tan d Peak)
  • Decomposition Temperature, IPC-TM-650.2.4.24.6, 5% weight loss; TGA
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Park Aerospace, former Park Electrochemical Corp.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.