| DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ionomer. Appeel® 72D727 is a modified ethylene vinyl acetate polymer available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Appeel® 72D727 resin complies with Food and Drug Administration Regulation 21 CFR 177.1330 subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use. The temperature of use must not exceed 100C / 212F. This former DuPont product line is now a Dow product line. |