| Features: Good stiffness and impact resistance, minimal warpage, good top loading capability, high surface gloss. Applications: Aerosol overcaps, food containers, frozen food containers, seedling trays, berry boxes. Data provided by the manufacturer. |
| High Density Polyethylene |