Features: Very high mechanical strength; Very high rigidity (also at low temperature); Very high thermal stability; Very high creep resistance; Very high dimensional stability; Very high radiation resistance; Very high hydrolysis resistance; Relatively low notch impact strength; Low resistance to acetone
Applications: Bearing shells; Piston rings; Valve seats; Gears; Seals; Aviation; Cog wheels; Pump vanes; Fittings; Plug connectors for the chromatography; Wafer carriers; Semiconductor industry