MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB GreenCoat® Hiarc Max Color Coated Steel
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: GreenCoat Hiarc Max color coated steel is available in regular and matte finishes. It is available in a wide range of colors inspired by Nordic nature. GreenCoat Hiarc Max is extremely durable (RC5 and Ruv5) and is specifically developed for fa?ades and cassettes. However, it can also be used in roofing applications. GreenCoat Hiarc Max color coated steel possesses excellent weather resistance properties and tolerates forming well. It offers extremely good corrosion resistance and is well suited for buildings in the harshest environments, like those near a coastline. Since GreenCoat Hiarc Max products offer a coating containing fluorine, the surface stays cleaner compared to other products. The coating is also easy to clean due to the hard surface. The reverse side of the sheet is painted with a two-layer grey backside coating. GreenCoat Hiarc Max complies with current REACH regulations and is fully chromate-free. SSAB’s color coated steels are all manufactured according to EN 10169. GreenCoat and Hiarc are trademarks of the SSAB group of companies.

Data provided by SSAB.

Vendors:
Available Properties
  • Thickness, Reverse Side Coating; Thickness (primer + top coat)
  • Thickness, Matt, Coating thickness, nominal (primer + top coat)
  • Thickness, Regular, Coating thickness, nominal (primer + top coat)
  • Thickness, Matt, steel thickness
  • Thickness, Regular, steel thickness
  • Maximum Service Temperature, Air, Matt
  • Maximum Service Temperature, Air, Regular
  • Gloss, Matt
  • Gloss, Regular
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.