MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
China-Yixing Longly Refractories Seggar Semi-Corundum-Mullite
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractoriness, thermal shock stability (Temperature-resistance degeneration urgency), high temperature strength, excellent corrosion resistance, anti-permeability slag strong, expansion coefficient of small, low creep, no chipping, not creaking easily, the use of stability, is the ideal tool to use high-temperature kilns furniture, to adapt to a variety atmosphere of conditions, in the use of high-temperature furnace; widely used in 95, 99 alumina ceramic and zirconia ceramic and fluorescent materials, powder metallurgy, electronic ceramics, magnetic materials, ceramic powders of high-temperature sintering.

Applications: For ceramic powders, electronic ceramics, powder metallurgy, magnetic materials, such as high-temperature sintering.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors:
Available Properties
  • Density
  • Porosity, Apparent
  • Flexural Strength, high temp bending
  • Flexural Strength, cold bending
  • Compressive Strength, Ambient
  • Maximum Service Temperature, Air
  • Al2O3
  • Fe2O3
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
China-Yixing Longly Refractories Co. Ltd

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.