MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Syensqo (Solvay Specialty Polymers) Ixan® PVS 827 PVDC
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: Ixan® PVS 827 is a ready-to-process PVDC based premix of low viscosity formulated to offer very good thermal stability as well as very good oxygen and water vapor barrier properties.
It is suitable for both extrusion and co-extrusion processes and is particularly recommended for use as barrier layers in multilayer food packaging films (heat shrinkable or not). This grade is especially dedicated to cheese & meat packaging applications.

Ixan® PVS 827 is compliant with FDA and EU 10/2011 requirements and is supplied as an off-white, free-flowing powder.

Applications: Food Packaging

Features: Moisture Barrier; Oxygen Barrier

PROCESSING
- As supplied, Ixan® PVS 827 is formulated for the extrusion or the coextrusion of multilayer barrier films. It can be processed by extrusion using machine designs that allow streamlined plastic flow in order to minimize the risk of plastic hold-up in the equipment.

- Regarding construction materials for the machine, Solvay Recommends that the parts in contact with the melt PVDC have high corrosion resistance and contain no catalytic materials (see below), i.e. those made of high Ni alloys like Xaloy®, Duranickel®, Colmonoy®, or Hastelloy®.

- It is essential that the temperature of Ixan® PVS 827 melt is kept below 180°C and the residence time is minimized.

- Thermal degradation during melt processing will release hydrogen chloride (HCl) gas. This reaction is catalyzed by the presence of Iron (Fe), Copper (Cu), and Zinc (Zn).

STORAGE
- Keep in a well-ventilated and dry place
- Do not store in heat or direct sunlight
- Keep only in the original package at a temperature not exceeding 40°C

ISO CERTIFICATION
The implemented management system for the production, internal transfer and delivery, design and development of Ixan® vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ISO 1183
  • Apparent Bulk Density, ISO 60
  • Particle Size
  • Oxygen Transmission Rate, ASTM D3985, 85% RH
  • Viscosity, ASTM D3835, Melt
  • Melting Point
  • FDA, and EU 10/2011
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.