| Good corrosion resistance and low coefficient-of-friction provides good metal-to-metal wear protection (not involving much impact). For bushings, knives and cams. Finished by grinding. Method of Application: Spraywelder, Fusewelder, PTA, HVOF Information provided by Wall Colmonoy Corporation. |