MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Ultra-Clean Spindle Oil ISO Grade 10
Categories: Fluid; Lubricant

Material Notes: Ultra-Clean Spindle Oil is a premium quality spindle bearing oil developed primarily for use in high-speed CNC milling machines and other machine tools that require an ultra-clean spindle oil. It meets the performance requirements of leading manufacturers of high-speed CNC milling machines. It also is recommended for use in textile machinery. Ultra-Clean Spindle Oil is formulated to provide excellent wear protection, protection against rust and corrosion, and resistance to foaming. It has excellent oxidation resistance and thermal stability at high temperatures to minimize deposits and provide longservice life. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foam buildup. It has the added advantage of fine filtration to a typical ISO Cleanliness Code of 17/15/11 for use in hydraulic systems with tight tolerances where particle contamination can cause operational problems.

Applications:

  • Horizontal, vertical, bed-type, knee-type and turret-type CNC milling machines, especially where particle contamination can cause operational problems
  • High-speed needle and spindle bearings in industrial, agricultural and textile machinery
  • Low-pressure hydraulic systems that require a low-viscosity oil
Features/Benefits:
  • Excellent oxidation resistance and thermal stability
  • Long service life for reduced operating and maintenance costs
  • Protects against wear
  • Excellent oiliness characteristics (ISO VG 2)
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Excellent low-temperature performance
  • Clear color
  • Non-staining
  • Quick foam release
  • Meets ISO Cleanliness Code rating of 17/15/11

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • ASTM Color, ASTM D1500
  • Total Acid Number, ASTM D974, [mg KOH/g]
  • Four Ball Wear, ASTM D2266, Scar Diameter
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.