MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Solvay FM® 6555-1 Ester Syntactic Core
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: FM® 6555-1 is a cyanate ester syntactic core material. It was designed as a cost and weight saving alternative in the manufacture of thin, stiffness critical composite panels for low dielectric applications and satellite structures. FM 6555-1 syntactic core is based on CYCOM® 5575-2 glass and quartz cyanate ester prepregs, FM 2555 and FM 2525 structural film adhesives and FM 313-27C syntactic paste, providing a compatible family of products. FM 6555-1 is available in sheet or roll form (availability in roll form is dependent on product thickness).

Features & Benefits:

  • One of a family of compatible products based on second-generation cyanate ester chemistry
  • Significantly improved electrical properties versus epoxy and BMI systems
  • Excellent mechanical properties
  • Service temperature from -70 to 350°F (-57 to 177°C) wet
  • Simple thermoset processing
  • Product and application patents received
Applications:
  • Thin composite panels for low dielectric applications and space structures where weight and/or cost are critical

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, ASTM D792, Cured
  • Volatiles, ASTM D3530
  • Viscosity
  • Viscosity
  • Viscosity
  • Viscosity
  • Storage Temperature
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D638, dry
  • Flexural Strength, ASTM D790
  • Compressive Strength, ASTM D1621, wet
  • Compressive Strength, ASTM D1621, dry
  • Compressive Strength, ASTM D1621, dry
  • Dielectric Constant, ASTM D2520
  • Dielectric Loss Index
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, ASTM D1356
  • Cure Time
  • Gel Time, Hot plate
  • Gel Time, Hot plate
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.