| Emulprene 1006 is a hot emulsion styrene-butadiene copolymer, polymerized using a fatty acid emulsifier and coagulated with salt-acid. It is a very light color product stabilized with a non-staining antioxidant. Uses: Emulprene 1006 is recommended for light colored applications; for adhesives, tire white sidewalls, transport and transmission belts, sponge materials, sporting goods, flooring, colored shoe soles and heels. Information provided by Dynasol Group. |