MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets
Categories: Polymer; Thermoset; Phenolic

Material Notes: Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good mechanical strength and electrical properties for use in low-voltage applications. Foil on both sides to protect the surface during processing, transport and installation. The foil may subsequently be removed from the finished components

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 PF CP 203, DIN 7735 Hp 2061, NF C26 150 P&PO, NEMA LI 1 XX
Vendors:
Available Properties
  • Density, ISO 1183-A, 24h/23°C/50% RH
  • Water Absorption, ISO 62-1
  • Tensile Strength, ISO 527, 24h/23°C/50% RH
  • Flexural Strength, ISO 178, 24h/23°C/50% RH, Normal to laminate plane
  • Flexural Modulus, ISO 178, 24h/23°C/50% RH, Normal to laminate plane
  • Compressive Strength, ISO 604, 24h/23°C/50% RH, , Normal to laminate plane
  • Shear Strength, IEC 60893-2, Parallel, 24h/23°C/50% RH
  • Izod Impact, Notched (ISO), ISO 180/2A, Parallel, 24h/23°C/50% RH
  • Insulation Resistance, IEC 60167, after immersion in water for 24 hr at 23°C
  • Dielectric Constant, IEC 60250, 96h/105°C + 1h/23°C/20%RH
  • Dielectric Strength, IEC 60243-1, after 1 hour in oil, Parallel to laminate plane
  • Dielectric Strength, IEC 60243-1, after 1 hour in oil, Normal to laminate plane
  • Dissipation Factor, IEC 60250, 96h/105°C + 1h/23°C/20%RH
  • Comparative Tracking Index, IEC 60112, 24h/23°C/50% RH
  • Maximum Service Temperature, Air, IEC 60216
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.