| Hostacom EKC 330N LG NA2 SOUL is a low gloss, high melt flow, medium high flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin. It has an excellent impact/stiffness balance, good flowability properties and excellent scratch resistance that is typically used for interior automotive applications. Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Impact Modified; Low Gloss Information provided by LyondellBasell. |