MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP22 Two Component, Aluminum Filled, Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Easily machinable
  • Two component epoxy
  • One to one mix ratio
  • Exceptionally high compressive strength
  • Superior dimensional stability
  • Aluminum filled
Product Description: Master Bond EP22 is an aluminum filled, two component epoxy adhesive for high performance bonding, sealing and coating. It is formulated to cure at room temperature or more rapidly at elevated temperatures, with a noncritical one to one mix ratio by weight or volume. EP22 is especially noteworthy for its sterling machinability, great dimensional stability and exceptionally high compressive strength. It bonds well to metals, especially steel and aluminum, as well as ceramics, composites, rubbers and many plastics. It has good void filling properties. The cured epoxy responds well to thermal cycling and has fine chemical resistance when exposed to water, fuels and oils. Although it is aluminum filled, it is a respectable electrical insulator. The presence of aluminum also promotes lower shrinkage than most epoxy systems. EP22 has an operating temperature range of -60°F to +250°F. The color of Part A is gray and Part B is gray. Master Bond EP22 system is widely used in specialty OEM, aerospace, chemical processing and selected electronic applications. It can be cured in thicker sections, and in this context it has utility as a cost effective repair and maintenance formulation for a wide range of machinery, especially industrial process equipment.

Product Advantages:

  • Convenient mixing: forgiving one to one mix ratio by weight or volume
  • Easy to apply — adhesive spreads evenly and smoothly; non-drip viscosity
  • Ambient temperature curing imparts optimal chemical resistance and hardness
  • Forms tough bonds; resistant to thermal cycling
  • Bonds well to a variety of substrates
  • Superb resistance to oils, fuels and related chemicals

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.