MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP40TC Two component, thermally conductive, electrically insulative epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Easy to use
  • Exceptional toughness
  • Excellent bond strength
  • NASA low outgassing
Product Description: Master Bond EP40TC is a two component, thermally conductive, electrically isolating epoxy for bonding and sealing. It combines convenient processing with superior strength properties after curing. It is a moderate viscosity, flowable system with a forgiving 1 to 1 mix ratio by weight or volume, and a user friendly working life. EP40TC cures readily at ambient temperatures or more rapidly with heat. The optimum cure schedule is overnight at room temperature followed by 3-5 hours at 125°F to 150°F. The system has no solvents or diluents and offers low shrinkage upon curing. This epoxy bonds well to a wide range of substrates including metals, ceramics, composites and many plastics. Most compelling is its exceptionally high shear and peel strength. EP40TC has remarkable toughness as indicated by its high elongation of 60-70%. This translates into the ability to withstand the most rigorous thermal cycling as well as vibration and shock. It is able to transfer heat, without conducting electricity. In fact, the particle size of the filler material is notably small, the largest being 12-14 microns, with an average size of 3-4 microns. This allows for particularly thin bond lines which lowers thermal resistance. EP40TC has good chemical resistance to water, oils, cleaning agents, and fuels. The color of Part A is light gray and Part B is gray. The service temperature range is -100°F to +300°F. EP40TC is an intriguing option in a variety of applications where the profile outline above is desirable. These include high strength structural bonding, where the parts are subjected to aggressive thermal cycling. Other uses would be as hermetic seals in electronic packaging, in bonding, sealing and high vacuum environments, and bonding in semiconductor and battery applications.

Product Advantages:

  • Easy processing, 1:1 mix ratio
  • Long open time
  • Outstanding shear and peel strength
  • Very high elongation
  • Vacuum compatible

Information provided by Master Bond.

Vendors:
Available Properties
  • Viscosity, Part B, thixotropic
  • Viscosity, Mixed
  • Viscosity, Part A, thixotropic
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap shear, Al to Al
  • Peel Strength, T-peel strength, steel to steel
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Optimal: overnight at 75°F, plus 3-5 hours at 125-150°F
  • Cure Time, Option 2
  • Working Life, after mixing, 100 gram batch
  • Shelf Life, in syringes, in original, unopened containers
  • Shelf Life, in cans, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.