MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chemical Concepts Chem-Set™ RTV7595 SILICONE SEALANT
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Construction Grade

Material Notes: FAST CURE 1-PART INDUSTRIAL/CONSTRUCTION GRADE SILICONE SEALANT Sil-FlexFC (RTV 7595) is a one component, low modulus, neutral cure silicone sealant and adhesive. It is chemically formulated to increase production output due to its accelerated skin, tack and full cure times; ideal for fast prototyping, production assembly lines and quick jobsite installations. When fully cured, this unique VOC compliant formula offers UV stability and tenacious adhesion to most common construction substrates. This product is specifically formulated to offer all weather performance to meet today's Green Building Standards.

Features & Benefits: Fast Cure, Excellent Adhesion, Non - Corrosive, Low Odor, 50% Movement Capability, Permanent Flexibility, Excellent Weatherability, Low Odor, VOC Compliant, Non Flammable, Waterproof

Applications: Sealing Openings & Exterior Surfaces, HVAC/ R Plumbing, Roofing, Kitchen & Bath, Countertops, Sanitary Seals, Precast Concrete, Industrial Gaskets, Transportation Seals, Marine Cabins, Appliance Trim & Parts, Interior/Exterior, Above Grade

MEETS SPECIFICATIONS: ASTM C920 Type S, NS, Class 50, TT-S-00230C, TT-S-01543A, MIL-A-46106A, AAMA 808.3, 805.2, 803.3 (Type I), 802.3 (Type II); UL Recognized Component.

AVAILABLE COLORS: Clear, White, Black, Aluminum (custom colors available upon request).

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.