MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Redwood Plastics Redco™ UHMW-PE REPROCESSED
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Redco™ Reprocessed UHMW is a blend of Virgin and Reprocessed polyethylene resulting in a cost effective alternative to Virgin UHMW. Redco™ Reprocessed UHMW is recommended for wear strip applications that do not require FDA approval.

Standard Color: Black, Green & Yellow

Typical Applications: Wear strip, channel, hold down wheels, slides, bearing blocks, wear rails, chute liners, hopper liners, wear shoes/ guides, low pressure gears, flights, light duty pulleys, dock fenders/pads, skate wheels, rollers, slider blocks, outrigger pads, etc.

Information provided by Redwood Plastics and Rubber

Vendors:
Available Properties
  • Density, ASTM D 792
  • Hardness, Rockwell R, ASTM D 785
  • Hardness, Shore D, ASTM D 2240
  • Tensile Strength, ASTM D 638, 2 in./min
  • Tensile Strength, Yield, ASTM D 638, 2 in./min
  • Elongation at Break, ASTM D 638, 2 in./min
  • Tensile Modulus, ASTM D 638, 2 in./min
  • Flexural Modulus, ASTM D 790
  • Izod Impact, Notched (ISO), ASTM D 256A
  • Coefficient of Friction, Dynamic, ASTM D 1894, Against Cr-Plated Steel
  • Coefficient of Friction, Static, ASTM D 1894, Against Cr-Plated Steel
  • Abrasion, Sand Slurry, Index (Relative To Steel At 100)
  • CTE, linear, ASTM D 696
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.