MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
United Initiators BENOX® L-40LV Dibenzoylperoxide
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: BENOX® L-40LV is a low viscosity, sprayable dispersion of dibenzoyl peroxide. BENOX®L-40LV is specifically designed for use in “curing” unsaturated polyester and vinyl ester resins and offers the following advantages:
  • Low water content
  • Faster gel to peak than MEKP systems
  • Lower exotherm than MEKP systems
  • Less “packing” in spray equipment designed/modified for spraying dibenzoyl peroxide dispersions
  • More stable and less separation than the common BPO dispersions on the market
  • Less viscosity drift
BENOX®L-40LV may also be used as a polymerization initiator for vinyl monomers, (e.g. styrene, acrylate, etc.).

CAS#94-36-0

Information provided by United Initiators.

Vendors:
Available Properties
  • Density
  • Brookfield Viscosity, HBT #4spindle 50 rpm
  • Storage Temperature
  • Critical Temperature, SADT
  • Shelf Life
  • Oxygen, O, Active
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.