| CirculenRecover PPC EKG 3539 NA TX7 BLK is a 15% glass fiber reinforced polypropylene compound, which contains recycled polypropylene resins. It has high stiffness and good impact resistance. It is typically used for mold-in color interior trim applications. Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Impact Resistance; Good Processability; Good UV Resistance; High Stiffness Information provided by LyondellBasell. |