MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Sandvik Bioline Cored wire
Categories: Metal; Nonferrous Metal

Material Notes: Sandvik Bioline cored wire (SBCW) is a composite wire consisting of a Sandvik Bioline F562 CoCrMo alloy shell and a secondary alloy as the core material. The core material is typically pure silver (Ag) to promote increased conductivity relative to solid Sandvik Bioline F562. However, other core materials such as platinum (Pt), gold (Au) and tantalum (Ta) can be selected in order to increase the radiopacity or provide other unique combinations of properties to the composite wire. The standard core dimension is 25% by area, however other core sizes can be considered. The outer component is characterized by:
  • Excellent corrosion resistance
  • Excellent fatigue properties
  • High strength combined with good ductility
The inner silver core provides:
  • High electrical efficiency
  • Electrical conductivity
  • Low electrical resistance.
Sandvik Bioline cored wire can be used for cochlear implants, pacemaker, defibrillator leads and varicose vein surgery devices.

Information provided by Sandvik

Vendors:
Available Properties
  • Tensile Strength, Ultimate, 0% CW, 45 Silver CSA
  • Tensile Strength, Ultimate, 0% CW, 40 Silver CSA
  • Tensile Strength, Ultimate, 0% CW, 35 Silver CSA
  • Tensile Strength, Ultimate, 0% CW, 30 Silver CSA
  • Tensile Strength, Ultimate, 20% CW, 45 Silver CSA
  • Tensile Strength, Ultimate, 0% CW, 25 Silver CSA
  • Tensile Strength, Ultimate, 30% CW, 45 Silver CSA
  • Tensile Strength, Ultimate, 20% CW, 40 Silver CSA
  • Tensile Strength, Ultimate, 40% CW, 45 Silver CSA
  • Tensile Strength, Ultimate, 30% CW, 40 Silver CSA
  • Tensile Strength, Ultimate, 20% CW, 35 Silver CSA
  • Tensile Strength, Ultimate, 50% CW, 45 Silver CSA
  • Tensile Strength, Ultimate, 60% CW, 45 Silver CSA
  • Tensile Strength, Ultimate, 40% CW, 40 Silver CSA
  • Tensile Strength, Ultimate, 30% CW, 35 Silver CSA
  • Tensile Strength, Ultimate, 20% CW, 30 Silver CSA
  • Tensile Strength, Ultimate, 50% CW, 40 Silver CSA
  • Tensile Strength, Ultimate, 40% CW, 35 Silver CSA
  • Tensile Strength, Ultimate, 20% CW, 25 Silver CSA
  • Tensile Strength, Ultimate, 60% CW, 40 Silver CSA
  • Tensile Strength, Ultimate, 30% CW, 30 Silver CSA
  • Tensile Strength, Ultimate, 50% CW, 35 Silver CSA
  • Tensile Strength, Ultimate, 40% CW, 30 Silver CSA
  • Tensile Strength, Ultimate, 30% CW, 25 Silver CSA
  • Tensile Strength, Ultimate, 60% CW, 35 Silver CSA
  • Tensile Strength, Ultimate, 50% CW, 30 Silver CSA
  • Tensile Strength, Ultimate, 40% CW, 25 Silver CSA
  • Tensile Strength, Ultimate, 60% CW, 30 Silver CSA
  • Tensile Strength, Ultimate, 50% CW, 25 Silver CSA
  • Tensile Strength, Ultimate, 60% CW, 25 Silver CSA
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.