MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
NatureWorks® Ingeo™ 2500HP Extrusion Grade PLA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Ingeo 2500HP is a high viscosity product from NatureWorks LLC, designed for extrusion applications. It is designed to crystallize during processing, leading to higher heat deflection temperatures in opaque applications. See table at right for properties.

Applications: The variety of products made with 2500HP is widely varied and growing. Applications include crystalline sheet for cards, graphic arts and signage.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Viscosity Measurement, ASTM D5225, RV measured at 1.0 g/dL in chloroform at 30°C
  • Linear Mold Shrinkage, molded amorphous with 26°C mold temperature
  • Linear Mold Shrinkage, molded crystalline with 120°C mold temperature
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638, molded amorphous with 26°C mold temperature
  • Tensile Strength, Yield, ASTM D638, molded crystalline with 120°C mold temperature(
  • Elongation at Break, ASTM D638, molded amorphous with 26°C mold temperature
  • Elongation at Break, ASTM D638, molded crystalline with 120°C mold temperature(
  • Flexural Strength, ASTM D790, molded amorphous with 26°C mold temperature
  • Flexural Strength, ASTM D790, molded crystalline with 120°C mold temperature
  • Flexural Modulus, ASTM D790, molded amorphous with 26°C mold temperature
  • Flexural Modulus, ASTM D790, molded crystalline with 120°C mold temperature
  • Izod Impact, Notched, ASTM D256, molded amorphous with 26°C mold temperature
  • Izod Impact, Notched, ASTM D256, molded crystalline with 120°C mold temperature(
  • Melting Point, Peak crystalline melting point, molded crystalline with 120°C mold temperature
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM E2092, molded amorphous with 26°C mold temperature
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM E2092, molded crystalline with 120°C mold temperature
  • Transmission, Visible, Thickness Unknown
  • Processing Temperature, Compression Section
  • Processing Temperature, Metering Section
  • Feed Temperature, Throat
  • Feed Temperature
  • Adapter Temperature
  • Die Temperature
  • Melt Temperature
  • Moisture Content
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
NatureWorks LLC

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.