MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Northstar Polymers GK-22R Polyurethane Gel Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: GK-22R is one of the formulas specifically formulated for manufacturing “sticky pads” or “reusable Pressure Sensitive Adhesives (PSA)” with the liquid resin casting process. The cured products have stronger adhesion property than the other sticky pad formula we carry, GK-7. The material can be processed at near room temperature*, and can be manually processed for small batches. It can also be processed with an inline meter mixing equipment for high volume productions. The cured material is intrinsically sticky without the use of tackifier resin. The product can be applied to and removed from solid surfaces multiple times. A film made of GK-22R retains a sticky surface indefinitely. When the surface is contaminated with dust and oil, it can easily be washed with soap and water to regain the stickiness. The cured film is soft and flexible but fairly strong to resist cut and tear. The stickiness can be adjusted by blending part-B and part-C components. A higher part-B ratio makes a product with lower adhesion strength, a higher part-C makes a product with higher adhesion strength. After the ratio to make the desired adhesion level is determined, the part-B/C blend can be mixed with part-A to make the product. The chart on right is the adhesion properties of GK-22R and GK-7 made into various adhesion levels tested with our in-house test method. The value is “pounds of force to delaminate 1” x 2” area adhered to TPE film (as shown in the picture above). GK-22R has a higher adhesion strength range than typical sticky pad products used in cellphone holders and other common sticky pad products. The GK-7#2 in this chart is close to typical sticky pad products.

#1 ---- 100: 0 = part-B : part-C 5.2 LBS
#2 ---- 75: 25 = part-B : part-C 5.4 LBS
#3 ---- 50: 50 = part-B : part-C 5.9 LBS
#4 ---- 25: 75 = part-B : part-C 6.5 LBS
#5 ---- 0: 100 = part-B : part-C 7.4 LBS (cohesion failure)

Designations
System Name: GK-22R
Part-A: MPG-055
Part-B: PPB-174
Part-C: PPD-174

Mixing ratio: Part-A: Part-(B/C) = 30: 100 by volume
Part-A: Part-(B/C) = 100: 312 by weight

Information provided by Northstar Polymers

Vendors:
Available Properties
  • Specific Gravity, Part-B Component
  • Specific Gravity, Part-C Component
  • Specific Gravity, Part-A Component
  • Viscosity, Part-B Component
  • Viscosity, Part-C Component
  • Viscosity, Part-A Component
  • Viscosity, Part-A Component
  • Viscosity, Part-A Component
  • Viscosity, Part-A Component
  • Viscosity, Part-A Component
  • Viscosity, Part-A Component
  • Viscosity, Part-A Component
  • Hardness, Shore OO, GK-22R#4
  • Hardness, Shore OO, GK-22R#3
  • Hardness, Shore OO, GK-22R#2
  • Hardness, Shore OO, GK-22R#1
  • Tensile Strength, GK-22R#4
  • Tensile Strength, GK-22R#2
  • Tensile Strength, GK-22R#3
  • Tensile Strength, GK-22R#1
  • Elongation at Break, GK-22R#1
  • Elongation at Break, GK-22R#2
  • Elongation at Break, GK-22R#3
  • Elongation at Break, GK-22R#4
  • Processing Temperature, Part-B Ambient
  • Processing Temperature, Part-A
  • Mold Temperature
  • Cure Time, Demolding
  • Cure Time, Complete
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.