MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP21TDCF-3 is a two component epoxy for high performance bonding and sealing. It is formulated to cure rapidly at room temperature or faster at elevated temperatures. It has a non-critical mix ratio of one to one by weight or volume. The faster cure allows for a shortened fixture time. Once cured, EP21TDCF-3 has excellent toughness. This gives the system outstanding mechanical shock resistance along with superior thermal cycling capabilities—even when bonding dissimilar substrates. It has a good blend of physical properties including high shear and peel strengths. It bonds well to a wide variety of substrates, including metals, glass, ceramics and many rubbers and plastics. EP21TDCF-3 has the ability to withstand an array of chemicals, including water, fuels and oils, over the service temperature range of -100°F to +250°F. It is 100% reactive without any solvents or diluents. The hardened adhesive is an excellent electrical insulator. The color of Part A is gray and Part B is amber. EP21TDCF-3 is a versatile, exceptionally strong, user friendly system that is widely used in the OEM, aerospace, electronic, electrical and related industries.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio.
  • Easy application, higher viscosity, thixotropic system.
  • Rapid curing at room temperature; shorter fixturing time.
  • Bonds well to a variety of substrates.
  • Noteworthy resistance to vibration, shock and thermal cycling.
  • Superior shear and peel strengths.
  • Good chemical resistance to water, fuels and oils.

Information provided by MasterBond®

Vendors:
Available Properties
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Shear Strength, Al/Al, Bond
  • Peel Strength, T-peel
  • Volume Resistivity
  • Dielectric Constant
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram mass
  • Shelf Life, in unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.