Temper: Soft Anneal Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed Common Fabrication Processes: Bending; Forming; Machining Typical Uses: Bourdon Tubes; Condenser Tube Plates; Condenser Tubes; Distiller Tubes; Evaporator Tubing; Ferrules; Heat Exchanger Tubing; Oil Well Pump Liner; Strainers Applicable Specifications: Condenser & Heat Exchanger Tube with Integral Fins – ASTM B956/B956M, Welded ASME SB956; Heat Exchanger Tube – Welded ASTM B543/B543M, Welded ASME SB543; Plate – ASTM B432; Plate & Sheet – for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M, for Pressure Vessels, Condensers & Heat Exchangers ASME SB171; Seamless Condenser Tube & Ferrule Stock – ASTM B111/B111M, ASME SB111; Seamless Heat Exchanger and Condenser Tube - U-Bend ASME SB395, with Integral Fins ASTM B359/B359M, U-Bend ASTM B395/B395M, with Integral Fins ASME SB359; Seamless Tube – Brass ASTMB135, Brass ASME SB135; Tube - Seamless (Metric) ASTM B135/B135M |