MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Industeel Superplast® Stainless Mold Steel
Categories: Metal; Ferrous Metal; Stainless Steel; Tool Steel; Mold Steel

Material Notes: SUPERPLAST® Stainless is a specially designed steel for plastic mould bases providing improved performances compared to standard grades such as 1.2085. SUPERPLAST® Stainless offers improved machinability, improved consistency and weldability, and increased thermal conductivity. Moreover, thanks to its low Carbon and 13% Chromium content, SUPERPLAST® Stainless ensures a good corrosion resistance (atmospheric as well as from acidic polymers). SUPERPLAST® Stainless offers significantly improved machinability (tool life and chip removal) when compared to 1.2085 commonly used for this application. The steel provides also an improved dimensional stability after machining, thanks to its balanced chemical composition and special heat treatment. Nevertheless, SUPERPLAST® is not recommended for texturing and polishing.

Vendors:
Available Properties
  • Hardness, Brinell, 40 mm from surface
  • Hardness, Brinell, 60 mm from surface
  • Hardness, Brinell, 20 mm from surface
  • Hardness, Brinell, 0 mm from surface
  • Hardness, Brinell, 80 mm from surface
  • Hardness, Brinell, 105 mm from surface
  • Hardness, Brinell, 108 mm from surface
  • Hardness, Brinell, 100 mm from surface
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.