Description: When the silk fiber is solubilized into an aqueous fibroin solution, it can be used as a basic material for preparing different silk fibroin materials such as gels, bio-scaffolds, nano/microspheres, membranes, as well as porous scaffolds for tissue engineering studies. It can also be used as an additive of protein in cell culture medium. Application: This product is manufactured in a manner to maximally preserve the molecular weight and structure of natural regenerated silk fibroin (a-helix or random coil structure). Information provided by Matexcel |