MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP62-1HTMed Two component epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Long open time at room temperature
  • Cures at moderately elevated temperatures
  • Superb physical strength profile
  • Passes ISO 10993-5
Product Description: Master Bond EP62-1HTMed is a two component epoxy system with a long working life at ambient temperature. The mix ratio is a forgiving 100 to 5 by weight. Upon mixing, it is a moderate viscosity system that flows well. The working life of 100 grams is 12-24 hours at room temperature. The cure schedule options are as follows, 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. However to obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is strongly recommended. The epoxy contains no solvents or diluents and has low shrinkage upon cure. The system bonds well to a wide variety of substrates such as metals, plastics, rubbers, ceramics and composites. Upon curing with the optimum schedule, EP62-1HTMed excels in combining high temperature resistance along with the ability to withstand repeated sterilization and many aggressive chemicals. It has a high glass transition temperature (see below). EP62-1HTMed is a dependable electrical insulating material. The service temperature range is -60°F to +450°F. The color of Part A is clear and Part B is dark brown. It is especially well suited for applications where harsh sterilants are being employed.

Product Advantages:

  • Very long working life
  • Good flow properties
  • Versatile curing schedules
  • Highly resistant to chemicals
  • Withstands repeated sterilization including autoclaving

Information provided by Master Bond.

Vendors:
Available Properties
  • Viscosity, Mixed
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap shear, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Cure Time, Optimum, post cure
  • Working Life, after mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.