| Hostacom TKC 2007N NA HF 82V TS is a high melt flow, 5% talc filled thermoplastic elastomeric olefin (TEO) resin. It is an impact modified grade that is typically used for interior applications that require excellent impact stiffness balance, excellent flowability properties, and very good scratch performance. Status: Developmental Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Flow; Good Impact Resistance; Good Moldability; Good Processability; Good Stiffness; Scratch Resistant Information provided by LyondellBasell. |