| PPS, linear, reinforced with 30% high-performance carbon fiber. For extreme strength and stiffness even at high temperatures. Very good wear resistance in sliding and friction applications. Properties: dimensionally stable, good chemical resistance, Good electrical properties, good aging behavior, good fire behavior, high continuous used temperature, High strength, High stiffness, semi-crystalline, high continuous used temperature Information provided by BARLOG plastics GmbH. |