| Graphene additive can be easily dispersed into admixture and additive formulations or water prior to mixing with cement, sand and aggregates, similar to any typical reagent or additive. With dosage rates as low as 0.01% of total concrete mix, a small amount of graphene additives goes a long way when it comes to enhancing strength, durability and multifunctionality. This enables thinner, lighter concrete products with improved tensile and compressive strength, reducing the carbon footprint of construction. Thisproduct also can be used across many other applications, such as paints, inks, latex, polymer and cement composites.Application: Sectors Construction, automotive, leisure products, textiles, coatings Morphology: Black Liquid |
| GRA-A001; Graphene Additives for Construction; graphene cement, graphene concrete |