MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Total PPH 3721WZ Polypropylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: High flow reactor homopolymer with a high level of antistat

High Flow - FINA 3721WZ is designed with high flow characteristics for ease of filling thin wall parts.

High Antistat - FINA 3721WZ is engineered with a high level of antistat for shelf cleanliness and mold release.

FDA - FINA 3721WZ complies with all applicable FDA regulations for food contact applications.

Nucleation - FINA 3721WZ is nucleated to provide fast cycle time and improve contact clarity in thin wall, multi-cavity molds.

Recommended Applications - FINA 3721WZ is ideal for caps, closures, cutlery, and other thin wall multi-cavity applications.

Processing - FINA 3721WZ resin processes on conventional injection molding equipment with typical melt temperatures of 390- 450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238L
  • Hardness, Rockwell R, ASTM D288A
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Modulus of Elasticity, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256A
  • Izod Impact, Unnotched, ASTM D256A
  • Melting Point, DSC
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Melt Temperature, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.