CDA 102 is a fluid filler metal used for brazing of ferrous and nickel based alloys in particular steel, stainless steel and copper-nickel alloys. This alloy is typically used in a furnace braze applications without the use of flux. CDA 102 is a free flowing filler metal that exhibits good wetting characteristics on ferrous and nickel based materials. Maximum strength and joint integrity are obtained where joint clearance falls within the range of 0.000 in. - 0.001 in. (0.000 – 0.025 mm) per side. The properties of a brazed joint are dependent upon numerous factors including base metal properties, joint design, metallurgical interaction between the base metal and the filler metal. Available forms: Wire, strip, engineered preforms, specialty preforms. Information provided by Lucas-Milhaupt. |
AWS A5.8M/A5.8 BCu-3; AMS 4501 (Sheet, Chemistry Only); AMS 4701 (Wire, Chemistry Only) |